【含量测定】 照气相色谱法(附录Ⅴ E)测定。
色谱条件与系统适用性试验 以硅酮(OV-17) 为固定相,涂布浓度为2 %;柱温为
265 ℃。理论板数按维生素E峰计算应不低于500 ,维生素E峰与内标物质峰的分离度
应大于2 。
校正因子测定 取正三十二烷适量,加正己烷溶解并稀释成每1ml 中含 1.0mg的溶
液,摇匀,作为内标溶液。另取维生素E对照品约20mg,精密称定,置棕色具塞锥形瓶
中,精密加入内标溶液10ml,密塞,振摇使溶解;取1 ~3μl注入气相色谱仪,计算校
正因子。
测定法 取本品约20mg,精密称定,置棕色具塞锥形瓶中,精密加入内标溶液10ml
,密塞,振摇使溶解;取1 ~3μl注入气相色谱仪,测定,计算,即得。
名称:不锈钢柱
规格:2m*3mm,60-80目
型号:1.5%OV-17/Shimalite W
编号:20230914001
*高温度:300°C
【 Content determination 】 Determine according to the gas chromatography method (Appendix V E).
Chromatographic conditions and system suitability tests were conducted using silicone (OV-17) as the stationary phase with a coating concentration of 2%; Column temperature is
265 ℃. The number of theoretical plates should not be less than 500 calculated based on the vitamin E peak, and the separation degree between the vitamin E peak and the internal standard substance peak should not be less than 500
Should be greater than 2.
Correction factor determination: Take an appropriate amount of n-hexane, dissolve it with n-hexane, and dilute it to a solution containing 1.0mg per 1ml
Shake well and use as the internal standard solution. Take approximately 20mg of vitamin E reference material, accurately weigh it, and place it in a brown conical flask with a stopper
Add 10ml of internal standard solution accurately, seal tightly, shake to dissolve; Take 1-3 μ Inject gas chromatograph, calculate and calibrate
Positive factor.
Determination method: Take approximately 20mg of this product, accurately weigh it, place it in a brown conical flask with a stopper, and accurately add 10ml of internal standard solution
Densify and shake to dissolve; Take 1-3 μ Inject into a gas chromatograph, measure, calculate, and obtain.
Name: Stainless steel column
Specification: 2m * 3mm, 60-80 mesh
Model: 1.5% OV-17/Shimalite W
No.: 20230914001